Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 125 MPa
18100 psi
CEN® Electronic Material CN Polyimide Film, 6 Mil Thickness
CEN®CN polyimide film is typical general-purpose polyimide film and has been used successfully in applications at temperatures as low as -269°C (-452°F) and as high as 400°C (752°F). CN film ca..