Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 10.9 MPa
1580 psi
Blown; ASTM D822
LyondellBasell Petrothene® NA373244 Low Density Polyethylene, Cast/Blown Film Grade
ApplicationsPetrothene NA373 is a series of homopolymer resins selected by customers for use in household film and other applications that require high clarity and good impact strength combined with..
Film Tensile Strength at Yield, MD 10.9 MPa
1580 psi
Blown; ASTM D822
LyondellBasell Petrothene® NA373242 Low Density Polyethylene, Cast/Blown Film Grade
ApplicationsPetrothene NA373 is a series of homopolymer resins selected by customers for use in household film and other applications that require high clarity and good impact strength combined with..