Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 10.6 MPa
1540 psi
ASTM D882
ExxonMobil Escorene® LL-3113 LLDPE/Hexene Premium High Strength 1.2 mil Film  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.An LLDPE hexene copolymer film resin. Films made from this resin have outstanding tensile, stiffness and toughness properties. These superior prope..