Film Tensile Strength at Yield, MD 15.9 MPa
2300 psi
ASTM D882
Dow DAF 780 Carpet Underlayment Adhesion Film
DAF 780 is a low melt point, coextruded film used to improve slip characteristics of polyurethane foam for carpet installation or other applications.Information provided by Dow
Film Tensile Strength at Yield, MD 15.9 MPa
2310 psi
ASTM D882
Bapolene® 122F Polyethylene, Film Grade
Bapolene LL122F is a general purpose LLDPE for blown film extrusion applications. This resin offers excellent tensile and toughness properties. Contains medium levels of slip/antiblock additives. ..
Film Tensile Strength at Yield, MD 15.9 MPa
2300 psi
ASTM D882
ExxonMobil Enable™ 35-05CH Metallocene Polyethylene Resin (European Grade)
Product Description: Enable 35-05CH is a metallocene ethylene-hexene copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact and ..