Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Yield, MD | 107.9 MPa | 15650 psi | 200°C (Stress at 5% Elongation (MD)); ASTM D882 |
UBE UPILEX 75S (75 micron) Polyimide Film Description: UPILEX, the ultra-high heat-resistant polyimide film, is the product of the polycondensation reaction between biphenyltetracarboxylic dianhydride (BPDA), of which process Ube Industries.. |