Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Limiting Pressure Velocity = 6200 psi-ft/min Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Limiting Pressure Velocity 0.217 MPa-m/sec
6200 psi-ft/min
Global EPP PET SL PET + Solid Lubricant
PET is an unreinforced, semi-crystalline thermoplastic polyester, demonstrating dimensional stability similar to acetal, combined with the comparable wear resistance of nylon. Heavily loaded mechani..