Polymer Property : Limiting Pressure Velocity = 6000 psi-ft/min Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Limiting Pressure Velocity 0.0500 - 0.210 MPa-m/sec
1430 - 6000 psi-ft/min
Average value: 0.0852 MPa-m/sec Grade Count:38
Overview of materials for High Density Polyethylene (HDPE), Ultra High Molecular Weight
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Ultra High Molecular Weight". Each property range of values reported i..