Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Limiting Pressure Velocity | 0.175 MPa-m/sec | 5000 psi-ft/min | 4:1 safety factor applied; QTM 55007 |
Quadrant EPP Nylatron® MD PA6, Metal-detectable Nylon (ASTM Product Data Sheet) Data provided by Quadrant Engineering Plastic Products Broadest size range availability Good mechanical and electrical properties Ideal balance of strength and toughness Cast as finished parts and n.. |
|||
Limiting Pressure Velocity | 0.175 MPa-m/sec | 5000 psi-ft/min | 100 fpm |
Techmer ES Luriblend® TPX-HDPE-99018 Availability: North AmericaForms: Pellets)Features: Good Wear Resistance and Low FrictionProcessing Method: Injection MoldingTPCI# 8869115Information provided by TP Composites, Inc. |