Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Limiting Pressure Velocity | 3.53 MPa-m/sec | 101000 psi-ft/min | 0.1 m/sec; S45C |
UBE UPIMOL® SA101 Heat-Resistant Polyimide Shape Description: UPIMOL® SA101 is an excellent heat-resistant polyimide shape, based on Biphenyl tetracarboxilic dianhydride(BPDA) originally developed by UBE. UPIMOL® SA101 has improved high durabili.. |