Mechanical Properties Metric English Comments
Limiting Pressure Velocity 0.0420 - 0.0876 MPa-m/sec
1200 - 2500 psi-ft/min
Average value: 0.0642 MPa-m/sec Grade Count:14
Overview of materials for Polytetrafluoroethylene (PTFE), Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Extruded". Each property range of values reported is minimum and maximum..