Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Limiting Pressure Velocity | 2.21 MPa-m/sec | 63100 psi-ft/min | 0.5 m/sec; S45C |
UBE UPIMOL® S High Heat Polyimide Shape Description: Ube's UPIMOL is an exceptionally heat-resistant polyimide Shape. This product has the same molecular structure as UPILEX, an ultra-high heat-resistant polyimide film developed by Ub.. |