Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Limiting Pressure Velocity | 0.00441 - 0.00491 MPa-m/sec | 126 - 140 psi-ft/min | 30 m/min |
Polikim EFALON® C-25 PTFE, 25% Glass Filled C15 and C25 have less thermal expansion, higher wear resistance and less deformation under load compared to virgin Efalon® (PTFE). Applications: Seals, Seal rings, gaskets, valve sets, piston rings.. |