Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Limiting Pressure Velocity | 1.667 MPa-m/sec | 47580 psi-ft/min | v = 200m/min |
Wolf Kunststoff ZEDEX® ZX-410V7T A4T Polymer Alloy, Fiber Reinforced, Friction Modified Main Characteristics: Fiber-reinforced; Friction-modified; Very high stiffness (higher than that of fiber-reinforced PEEK); Very low thermal expansion coefficient; Low friction; High wear resistance.. |