Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Limiting Pressure Velocity | 1.50 MPa-m/sec | 42800 psi-ft/min | at 0.5 m/s |
Shell Carilon® DA6P2L10 Polyketone, High Performance Lubricated Injection Molding Grade
(discontinued **) Shell announced in Feb. 2000 that the Carilon product line is being discontinued. CARILON Polymer DA6P2L10 is a high-performance lubricated injection molding grade with mechanical properties which .. |
|||
Limiting Pressure Velocity | 1.50 MPa-m/sec | 42800 psi-ft/min | |
Kuraray Genestarâ„¢ G1352A-M41 Nylon, 35% Glass Filled Low friction reinforced injection grade.Main Features:Low friction coefficientAbrasion resistanceExamples of applications:Friction and wear applicationGear and wheel |
|||
Limiting Pressure Velocity | 1.50 MPa-m/sec | 42800 psi-ft/min | |
Trelleborg Sealing Solutions Turcite® TX Self-Lubricating Thermoplastic Rod Red color. Turcite® TX is engineered to handle moderate load, high speed applications. It exhibits an excellent surface finish when machined. It has a long service life and exceptionally low coe.. |