Polymer Property : Limiting Pressure Velocity = 1.40 MPa-m/sec Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Limiting Pressure Velocity 1.40 MPa-m/sec
40000 psi-ft/min
4:1 safety factor; QTM 55007
Quadrant EPP Duratron® PI D7015G PI Bearing Grade Polyimide (ASTM Product Data Sheet)
Limiting Pressure Velocity 1.40 MPa-m/sec
40000 psi-ft/min
4:1 safety factor; QTM 55007
Quadrant EPP Duratron® PAI T4301 Polyamide-imide, extruded bearing grade (ASTM Product Data Sheet)