Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Limiting Pressure Velocity | 0.0513 - 1.08 MPa-m/sec | 1460 - 30800 psi-ft/min | Average value: 0.297 MPa-m/sec Grade Count:4 |
Overview of materials for Acetal Homopolymer, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Unreinforced". Each property range of values reported is minimum and maximum values .. |