Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Limiting Pressure Velocity | 1.08 MPa-m/sec | 30800 psi-ft/min | pressure of 1 MPa |
Asahi Kasei Tenac® LT805 Acetal Homopolymer, Low Friction Grade