Mechanical Properties Metric English Comments
Limiting Pressure Velocity 0.640 MPa-m/sec
18300 psi-ft/min
Kuraray Genestarâ„¢ N1001D-U03 Nylon
Standard unreinforced extrusion grade. Main Features:Outstanding fuel barrierHeat resistanceExample of applications:Multi-layered fuel tube