Mechanical Properties Metric English Comments
Limiting Pressure Velocity 0.596 MPa-m/sec
17000 psi-ft/min
4:1 safety factor; QTM 55007
Quadrant EPP Nylatron® 703 XL Cast, Wear Resistant, Zero 'Stick-Slip' (ASTM Product Data Sheet)
Limiting Pressure Velocity 0.596 MPa-m/sec
17000 psi-ft/min
4:1 safety factor; QTM 55007
Quadrant EPP Semitron® ESd 490HR Static dissipative PEEK for use in test fixtures. Non-sloughing and low moisture absorption. (ASTM Product Data Sheet)
Limiting Pressure Velocity 0.596 - 1.54 MPa-m/sec
17000 - 44000 psi-ft/min
Average value: 0.690 MPa-m/sec Grade Count:8
Overview of materials for Nylon 66, Heat Stabilized
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Heat Stabilized". Each property range of values reported is minimum and maximum values of appr..
Limiting Pressure Velocity 0.596 MPa-m/sec
17000 psi-ft/min
10 fpm
Techmer ES Luriblend® PA6/6 GF30 TS1 BK 30% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: Heat Stabilizer, Silicone Lubricant and PTFE Lubricant(15%)Features: Lubricated, Good Wear R..
Limiting Pressure Velocity 0.596 MPa-m/sec
17000 psi-ft/min
1000 fpm
Techmer ES Luriblend® PA6/6 GF30 TS1 BK 30% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: Heat Stabilizer, Silicone Lubricant and PTFE Lubricant(15%)Features: Lubricated, Good Wear R..
Limiting Pressure Velocity 0.596 MPa-m/sec
17000 psi-ft/min
10 fpm
Techmer ES Luriblend® PA6/6 GF30 TS15 30% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: Heat Stabilizer, Silicone Lubricant and PTFE Lubricant(15%)Features: Lubricated, Good Wear R..
Limiting Pressure Velocity 0.596 MPa-m/sec
17000 psi-ft/min
1000 fpm
Techmer ES Luriblend® PA6/6 GF30 TS15 30% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: Heat Stabilizer, Silicone Lubricant and PTFE Lubricant(15%)Features: Lubricated, Good Wear R..
Limiting Pressure Velocity 0.596 MPa-m/sec
17000 psi-ft/min
10 fpm
Techmer ES Luriblend® PA6/6 GF33 TS15 33% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 33% Filler by WeightAdditive: Heat Stabilizer, Silicone Lubricant and PTFE Lubricant(15%)Features: Lubricated, Good Wear R..
Limiting Pressure Velocity 0.596 MPa-m/sec
17000 psi-ft/min
1000 fpm
Techmer ES Luriblend® PA6/6 GF33 TS15 33% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 33% Filler by WeightAdditive: Heat Stabilizer, Silicone Lubricant and PTFE Lubricant(15%)Features: Lubricated, Good Wear R..
Limiting Pressure Velocity 0.596 MPa-m/sec
17000 psi-ft/min
10 fpm
Techmer ES Luriblend® PA6/6 GF33 TS15 BK 33% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 33% Filler by WeightAdditive: Heat Stabilizer, Silicone Lubricant and PTFE Lubricant(15%)Features: Lubricated, Good Wear R..
Limiting Pressure Velocity 0.596 MPa-m/sec
17000 psi-ft/min
1000 fpm
Techmer ES Luriblend® PA6/6 GF33 TS15 BK 33% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 33% Filler by WeightAdditive: Heat Stabilizer, Silicone Lubricant and PTFE Lubricant(15%)Features: Lubricated, Good Wear R..
Limiting Pressure Velocity 0.596 MPa-m/sec
17000 psi-ft/min
4:1 safety factor; QTM 55007
Quadrant EPP Ketron® CM CA30 PEEK Polyetheretherketone, 30% carbon fiber reinforced, compression molded (ASTM Product Data Sheet)
Data provided by Quadrant Engineering Plastic Products Excellent chemical resistance Very low moisture absorption Inherently good wear and abrasion resistance Unaffected by continuous exposure to ho..