Polymer Property : Limiting Pressure Velocity = 0.150 MPa-m/sec Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Limiting Pressure Velocity 0.150 MPa-m/sec
4280 psi-ft/min
at 1 m/s unlubricated
Quadrant EPP Ertalon® LFX PA 6 + oil, cast (ISO Data)
This internally lubricated cast nylon 6 is self-lubricating in the real meaning of the word. Ertalon LFX, especially developed for unlubricated, highly loaded and slow moving parts applications, yie..
Limiting Pressure Velocity 0.150 MPa-m/sec
4280 psi-ft/min
at 0.1 m/s unlubricated
Quadrant EPP Ertalyte® PET, cast (ISO Data)
The specific properties of this virgin crystalline PET make it especially suitable for the manufacture of mechanical precision parts which have to sustain high loads and/or are subject to wear.
Limiting Pressure Velocity 0.150 MPa-m/sec
4280 psi-ft/min
without lubrication; MPC Test
Manifattura Cattaneo POM c Acetal
Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a.
Limiting Pressure Velocity 0.150 MPa-m/sec
4280 psi-ft/min
v = 100m/min
Wolf Kunststoff ZEDEX® ZX-530KF15 A5M Polymer Alloy
Main Characteristics: High elongation; High impact strength; Stress resistantApplications: Chemical Engineering; Laboratory Technology; Automitve Technology; Machine ToolsInformation provided by Zed..