Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Limiting Pressure Velocity | 0.0657 - 2.80 MPa-m/sec | 1880 - 79900 psi-ft/min | Average value: 1.40 MPa-m/sec Grade Count:10 |
Overview of materials for Polyetherimide (PEI) This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide". Each property range of values reported is minimum and maximum values of appropriate Mat.. |