Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 952 MPa @Strain 0.200 % |
138000 psi @Strain 0.200 % |
Transverse, typical |
TIMET TIMETAL® 62S Titanium Alloy (Ti-6Al-2Fe-0.1Si); Beta Forged Low Cost, Multipurpose Alloy. Tensile/toughness property data below for Beta Forged, RA material.Features: Properties and processing characteristics equivalent to or better than TIMETAL 6-4, but wi.. |