Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 517 - 655 MPa @Strain 0.200 %, Thickness <=25.4 mm |
75000 - 95000 psi @Strain 0.200 %, Thickness <=1.00 in |
Cold Drawn Bars |
Schmolz + Bickenbach UGIMA 303 UX® Stainless Steel Bar Description: 303 UGIMA UX® is an improved machining grade produced only by Ugitech, providing the ultimate level of machinability available in an austenitic stainless steel. 303 UGIMA UX® feat.. |
|||
Tensile Strength, Yield | 345 - 655 MPa @Strain 0.200 %, Thickness <=25.4 mm |
50000 - 95000 psi @Strain 0.200 %, Thickness <=1.00 in |
Cold Drawn Bars |
Schmolz + Bickenbach UGIMA® 316/316L Stainless Steel Bar Description: 316/316L UGIMA® is Ugitech’s improved machining grade produced only by Ugitech. It is identical in every way to regular 316L, except with respect to machinability. 316/316L UGIM.. |