Polymer Property : Tensile Strength, Yield = 9300 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 64.1 MPa

@Thickness 1.57 mm
9300 psi

@Thickness 0.0620 in
CW; ASTM D638
Industrial Laminates/Norplex NP159 Synthetic Fabric  (discontinued **)
Description: Woven aramid fiber fabric combined with high temperature phenolic resin. With a proper post baking procedure, NP159 will withstand continuous operation at 200° C. Material becomes brit..