Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 63.0 MPa @Strain 0.200 %, Temperature 980 °C |
9140 psi @Strain 0.200 %, Temperature 1800 °F |
|
Haynes X-750 Nickel Alloy Sheet and Strip (AMS 5598, UNS N07750) Haynes X-750 (UNS No. N07750) alloy is an age-hardenable, nickel-base superalloy with very good strength at temperatures up to about 1600°F (870°C). It is widely used as a wrought material for.. |