Mechanical Properties Metric English Comments
Tensile Strength, Yield 9.81 MPa

@Strain 300 %
1420 psi

@Strain 300 %
ASTM D412
SK Chemicals SKYTHANE® 185A R series Polyurethane
SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr..
Tensile Strength, Yield 9.81 MPa

@Strain 100 %
1420 psi

@Strain 100 %
ASTM D412
SK Chemicals SKYTHANE® R180A C series Polyurethane
SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr..
Tensile Strength, Yield 9.81 MPa

@Strain 300 %
1420 psi

@Strain 300 %
ASTM D412
SK Chemicals SKYTHANE® R180A C series Polyurethane
SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr..
Tensile Strength, Yield 9.81 MPa

@Strain 100 %
1420 psi

@Strain 100 %
ASTM D412
SK Chemicals SKYTHANE® 590A X series Polyurethane
SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr..
Tensile Strength, Yield 9.81 MPa

@Strain 100 %
1420 psi

@Strain 100 %
ASTM D412
SK Chemicals SKYTHANE® 392A S series Polyurethane
SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr..
Tensile Strength, Yield 9.81 MPa

@Strain 5.00 %
1420 psi

@Strain 5.00 %
ASTM D638
Samyang Triel® 5500 Thermoplastics Polyetherester Elastomer, General Extrusion
Excellent mechanical characteristics, elasticity, thermal resistance and chemical resistance.5500 is an extrusion grade.Information provided by Samyang.