Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 869 MPa

@Strain 0.200 %,
Temperature 199 °C
126000 psi

@Strain 0.200 %,
Temperature 390 °F
Longitudinal Tests from 3" rolled plate at 321 HB
EDRO RoyAlloy™ #6 Free Machining Stainless Holder Steel
RoyAlloy™ is a 400 series martensitic stainless steel supplied prehardened. RoyAlloy™ is characterized by excellent machinability, good corrosion resistance, uniform and consistent hardness in all..