Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 594 MPa @Temperature 649 °C, Time 11500 sec |
86200 psi @Temperature 1200 °F, Time 3.20 hour |
As Welded, Solution Annealed, and Aged; Base/Weld Fracture; 0.2% Offset |
Haynes 282® Nickel Alloy Autogenously Welded Sheet Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la.. |