Polymer Property : Tensile Strength, Yield = 81000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 558 MPa

@Temperature 23.9 °C
81000 psi

@Temperature 75.0 °F
0° Direction, Dry; ASTM D638 Type 1
Park Electrochemical Nelcote® E-722 Epoxy Prepreg, 285 Kevlar® Reinforced
Nelcote® E-722 is a modified 350°F cure epoxy system with excellent processing characteristics for vacuum bag, press, and autoclave molding.Key Features and Benefits:Epoxy resin system optimized f..
Tensile Strength, Yield 558 MPa

@Temperature 87.8 °C
81000 psi

@Temperature 190 °F
0° Direction, Dry; ASTM D638 Type 1
Park Electrochemical Nelcote® E-722 Epoxy Prepreg, 285 Kevlar® Reinforced
Nelcote® E-722 is a modified 350°F cure epoxy system with excellent processing characteristics for vacuum bag, press, and autoclave molding.Key Features and Benefits:Epoxy resin system optimized f..