Polymer Property : Tensile Strength, Yield = 80600 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 556 MPa

@Strain 0.200 %,
Temperature 800 °C
80600 psi

@Strain 0.200 %,
Temperature 1470 °F
Special Metals NIMONIC® alloy 91 Ni-Cr-Co Alloy
NIMONIC® alloy 91 is a wrought nickel-chromium-cobalt based alloy strengthened by additions of aluminum and titanium.This alloy is a modification of NIMONIC alloy 90, but has an increased chromium ..