Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 8.96 MPa @Strain 0.200 %, Temperature 1090 °C |
1300 psi @Strain 0.200 %, Temperature 2000 °F |
Longitudinal |
AK Steel NITRONIC® 19-D Duplex Stainless Steel AK Steel NITRONIC® 19D is a stainless steel with a mixed ferrite and austenite structure. This alloy provides high yield strength (65 ksi minimum {448 MPa}),