Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 8.398 MPa @Temperature 22.2 °C |
1218 psi @Temperature 72.0 °F |
Flatwise Tensile, 5 days @ 22°C/72°F, Conditioning: Dry; EN2243-4 |
Hexcel® Redux® 810 Two-Part Epoxy Paste Adhesive Redux® 810 is a multi-purpose, high shear and peel strength, two-part, toughened epoxy paste adhesive with corrosion-inhibiting properties.Features: Available in cartridges with a static mixer and .. |