Mechanical Properties Metric English Comments
Tensile Strength, Yield 793 MPa

@Treatment Temp. 427 °C,
Time 2.88e+7 sec
115000 psi

@Treatment Temp. 801 °F,
Time 8000 hour
0.2%. Room temp test after thermal exposure
Haynes Hastelloy® C-22HS™ Nickel Alloy Plate, Age-hardened
Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou..
Tensile Strength, Yield 793 MPa

@Temperature 25.0 °C
115000 psi

@Temperature 77.0 °F
90°, Dry
Hexcel® HexPly® 8552 Epoxy Matrix, A193-PW Fiber
Information provided by HexCel
Tensile Strength, Yield >= 793 MPa

@Strain 0.200 %
>= 115000 psi

@Strain 0.200 %
AMS 5598 aged, sheet
ATI Allegheny Ludlum Altemp® X-750 Nickel-Based superalloy
Characteristics: precipitation hardenable, high strength up to 1300°F, oxidation resistant up to 1800°F. Applications: aerospace, heat treatment fixtures, forming tools, extrusion dies.Information..