Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield >= 54.0 MPa

@Temperature 300 °C
>= 7830 psi

@Temperature 572 °F
PEAK Werkstoff DISPAL S250 Aluminum Alloy, AlSi20Fe5Ni2, Condition F
Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational..
Tensile Strength, Yield 54.0 MPa

@Temperature 23.0 °C
7830 psi

@Temperature 73.4 °F
50%RH; ISO 527
DuPont Performance Polymers Zytel® 151 NC010 Nylon 612  (Unverified Data**)
Zytel® 151 NC010 is a PA 612 resin.Information provided by DuPont Performance Polymers
Tensile Strength, Yield 54.0 MPa

@Temperature 23.0 °C
7830 psi

@Temperature 73.4 °F
50%RH; ISO 527
DuPont Performance Polymers Zytel® SC315 NC010 Nylon 612  (Unverified Data**)
Zytel® SC315 NC010 is an unreinforced, lubricated 612 polyamide suitable for injection molding. It has been developed for applications such as parts for the healthcare industry.Information provided..