Tensile Strength, Yield 538 MPa

@Temperature -196 °C
78000 psi

@Temperature -320 °F
Crucible Steel 20 Cb Plus Stainless Steel
Crucible 20 Cb Plus is a non-hardenable stabilized stainless steel with exceptional resistance to sulfuric, phosphoric, and nitric acid. This grade also has good resistance to stress corrosion crack..