Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 765 MPa @Temperature -55.0 °C |
111000 psi @Temperature -67.0 °F |
0°, Dry |
Hexcel® HexPly® 8552 Epoxy Matrix, A193-PW Fiber Information provided by HexCel |
|||
Tensile Strength, Yield | 765 MPa @Temperature 93.3 °C |
111000 psi @Temperature 200 °F |
90°, Dry |
Hexcel® HexPly® 8552 Epoxy Matrix, A193-PW Fiber Information provided by HexCel |
|||
Tensile Strength, Yield | 765 MPa @Strain 0.200 % |
111000 psi @Strain 0.200 % |
Longitudinal |
AK Steel 15-5 PH® Precipitation Hardening Stainless Steel, Condition H 1150-M AK Steel 15-5 PH® provides high strength, good corrosion resistance, good mechanical properties at temperatures up to 600°F (316°C), and good toughness in both base metal and welds. Short-time, .. |
|||
Tensile Strength, Yield | 765 MPa @Strain 0.200 % |
111000 psi @Strain 0.200 % |
Transverse |
AK Steel 15-5 PH® Precipitation Hardening Stainless Steel, Condition H 1150-M AK Steel 15-5 PH® provides high strength, good corrosion resistance, good mechanical properties at temperatures up to 600°F (316°C), and good toughness in both base metal and welds. Short-time, .. |