Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 5.20 MPa @Strain 100 % |
754 psi @Strain 100 % |
ASTM D412 |
GRECO ISOTHANE 3080AF Polyether TPU Resin ISOTHANE 3000F Series products are polyether based thermoplastic polyurethanes. They exhibit excellent hydrolytic resistance, fungus resistance, and low temperature performance properties. These pro.. |
|||
Tensile Strength, Yield | 5.20 MPa @Strain 100 % |
754 psi @Strain 100 % |
ASTM D412 |
GRECO ISOTHANE 2080A Poly(caprolactone)ester TPUÂ Resin ISOTHANE 2000 series products are polyester poly(caprolactone)ester based thermoplastic polyurethane. They exhibit excellent toughness, abrasive resistance, solvent resistance, and hydrolysis stabi.. |
|||
Tensile Strength, Yield | 5.20 MPa @Strain 100 % |
754 psi @Strain 100 % |
ASTM D-412 |
BASF Elastollan® C-78A Polyester Type Polyurethane Elastomer Processed by extrusion or injection molding. Elastollan C series of products are polyester-based thermoplastic polyurethanes that exhibit very good hydrolytic stability. They also exhibit excellen.. |
|||
Tensile Strength, Yield | 5.20 MPa @Strain 300 % |
754 psi @Strain 300 % |
ASTM D412 |
SK Chemicals SKYTHANE® 365A T series Polyurethane SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr.. |