Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 513 MPa @Temperature 71.0 °C |
74400 psi @Temperature 160 °F |
Wet |
Hexcel® HexPly® F593 Epoxy Resin, F3T584 Carbon Fabric Hexcel designation: F3T584-42"-F593; Fiber: Toray T-300/3kInformation provided by HexCel |