Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 71.7 MPa @Thickness 1.57 mm |
10400 psi @Thickness 0.0620 in |
CW; ASTM D638 |
Industrial Laminates/Norplex NP625 Paper Base Laminate Description: Paper phenolic grade with better moisture resistance than NP612. Requires less heat to punch and shear than NP611. |