Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 4.80 MPa

@Strain 100 %
696 psi

@Strain 100 %
ASTM D412
GRECO ISOTHANE 1180A Poly(adipate)ester TPU Resin
ISOTHANE 1100 series products are transparent grade, polyester poly(adipate)ester based thermoplastic polyurethanes. They exhibit good toughness, solvent resistance, easy processing, and high transp..
Tensile Strength, Yield 4.80 MPa

@Strain 100 %
696 psi

@Strain 100 %
ASTM D412
GRECO ISOTHANE 1075A Poly(adipate)ester TPU Resin
ISOTHANE 1000 series products are general purpose poly(adipate)ester based thermoplastic polyurethanes. They exhibit excellent toughness, abrasive resistance, and solvent resistance. These products ..
Tensile Strength, Yield 4.80 MPa

@Strain 100 %
696 psi

@Strain 100 %
ASTM D412
GRECO ISOTHANE 1080AF Poly(adipate)ester TPU Resin
ISOTHANE 1000 FDA series products are poly(adipate)ester based thermoplastic polyurethanes. They exhibit excellent toughness, abrasive resistance and solvent resistance. These products can be inject..
Tensile Strength, Yield 4.80 MPa

@Strain 100 %
696 psi

@Strain 100 %
ASTM D-412
BASF Elastollan® 1175A10W Wire & Cable Grade Polyurethane Elastomer
As with all TPU products this grade must be dried prior to processing.Information provided by BASF Corporation.
Tensile Strength, Yield 4.80 MPa

@Strain 100 %
696 psi

@Strain 100 %
ASTM D-412
BASF Elastollan® S80A Polyester Type Polyurethane Elastomer
Processed by extrusion or injection molding. Elastollan S series of products are polyester-based thermoplastic polyurethanes that exhibit good hydrolytic stability. They also exhibit good oil, fue..