Polymer Property : Tensile Strength, Yield = 676 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 676 MPa

@Temperature 82.2 °C
98000 psi

@Temperature 180 °F
0° Direction, Dry; Vacuum/Oven Cured; ASTM D3039-95
Park Electrochemical Nelcote® E-765 Epoxy Prepreg, T300 6K 5HS Reinforced
Nelcote® E-765 is a tough 250°F cure prepreg system designed to replace 350°F cure systems in aircraft structural applications. FAA-approved Design Allowable Databases are available upon request...
Tensile Strength, Yield 676 MPa

@Thickness 12.7 mm,
Temperature 20.0 °C
98000 psi

@Thickness 0.500 in,
Temperature 68.0 °F
0.2% offset
Haynes Ultimet® alloy, plate, GMAW weld (short)
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..