Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 447 MPa @Strain 0.200 %, Thickness 1.45 mm |
64800 psi @Strain 0.200 %, Thickness 0.0571 in |
|
Haynes Hastelloy® S alloy, flat products, solution heat-treated at 760°C (1400°F), aged 4000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
Tensile Strength, Yield | 447 MPa @Diameter 12.7 mm, Temperature 149 °C |
64800 psi @Diameter 0.500 in, Temperature 300 °F |
0.2% Offset |
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) All Weld Cruciform HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing.. |