Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 6.67 - 6.86 MPa @Strain 50.0 % |
967 - 996 psi @Strain 50.0 % |
ASTM D638 |
Samyang Triel® 5300 Thermoplastic Polyether Ester Elastomer TRIEL® resins offer superior mechanical properties, elasticities, heat and chemical resistance, which allow it to be widely used for electric/electronic equipments, automotive parts and outdoor rec.. |