Polymer Property : Tensile Strength, Yield = 6.20 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 6.20 MPa

@Strain 50.0 %
899 psi

@Strain 50.0 %
ASTM D412
GRECO ISOTHANE 3090A Polyether TPU Resin
ISOTHANE 3000 Series products are polyether based thermoplastic polyurethanes. They exhibit excellent hydrolytic resistance, fungus resistance, and low temperature performance properties. These prod..
Tensile Strength, Yield 6.20 MPa

@Strain 50.0 %
899 psi

@Strain 50.0 %
ASTM D412
GRECO ISOTHANE 3090AF Polyether TPU Resin
ISOTHANE 3000F Series products are polyether based thermoplastic polyurethanes. They exhibit excellent hydrolytic resistance, fungus resistance, and low temperature performance properties. These pro..
Tensile Strength, Yield 6.20 MPa

@Strain 50.0 %
899 psi

@Strain 50.0 %
ASTM D412
GRECO ISOTHANE 5090A Polyether TPU Resin
ISOTHANE 5000 Series products are polyether based thermoplastic polyurethanes. They exhibit excellent bio-compatibility, hydrolytic resistance, fungus resistance, and low temperature performance pro..
Tensile Strength, Yield 6.20 MPa

@Strain 100 %
899 psi

@Strain 100 %
ASTM D412
GRECO ISOTHANE 1085AF Poly(adipate)ester TPU Resin
ISOTHANE 1000 FDA series products are poly(adipate)ester based thermoplastic polyurethanes. They exhibit excellent toughness, abrasive resistance and solvent resistance. These products can be inject..