Polymer Property : Tensile Strength, Yield = 58.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 58.0 MPa

@Temperature 23.0 °C
8410 psi

@Temperature 73.4 °F
50%RH; ASTM D638
DuPont Performance Polymers Zytel® 101 NC010 Nylon 66  (Unverified Data**)
Zytel® 101 NC010 is a general purpose polyamide 66 resin for injection molding and extrusion.Information provided by DuPont Performance Polymers
Tensile Strength, Yield 58.0 MPa

@Strain 0.200 %,
Temperature 1095 °C
8410 psi

@Strain 0.200 %,
Temperature 2003 °F
Haynes 617 Nickel Alloy Plate
Haynes 617 alloy is a nickel-chromium-cobalt-molybdenum alloy with a good combination of metallurgical stability, strength, and oxidation resistance at high temperatures. The alloy is readily formed..