Polymer Property : Tensile Strength, Yield = 572 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 572 MPa

@Temperature -53.9 °C
83000 psi

@Temperature -65.0 °F
0° Direction, Dry; ASTM D638
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 120 E-Glass Reinforced
Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle..
Tensile Strength, Yield 572 MPa

@Strain 0.200 %,
Temperature 500 °C
83000 psi

@Strain 0.200 %,
Temperature 932 °F
Haynes Hastelloy® C-22HS™ Nickel Alloy Sheet, Cold-rolled, Solution Annealed, Age-hardened
Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou..