Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 570.0 MPa @Strain 0.200 % |
82670 psi @Strain 0.200 % |
after porcelain firing |
Wieland Porta P6 PFM Alloy Gold-platinum-palladium ceramic alloyApplications: crowns, short span bridges, long span bridges, telescopic and milling work, ceramic veneering, acrylic veneeringDental |