Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Yield = 56000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 386 MPa

@Temperature 177 °C
56000 psi

@Temperature 350 °F
0° Direction, Wet; ASTM D638 Type 1
Park Electrochemical Nelcote® P-670I Polyester Prepreg, 7781 E-Glass Reinforced
Nelcote® P-670I is a versatile, non-styrenated/low VOC polyester resin. P670I is used in a wide variety of applications including radomes, tooling and aircraft structures.Key Features and Benefits:..
Tensile Strength, Yield 386 MPa

@Temperature 23.9 °C
56000 psi

@Temperature 75.0 °F
0° Direction, Dry; ASTM D638
Park Electrochemical Nelcote® V-376 Cyanate Ester Epoxy Prepregs, 7781 E-Glass Reinforced
Nelcote® V-376 is a Cyanate Ester matrix providing excellent electrical and mechanical properties for harsh aircraft, shipboard, and undersea applications for Radomes, Antenna, and Reflectors. Simp..
Tensile Strength, Yield 386 MPa

@Diameter 12.7 mm,
Temperature 450 °C
56000 psi

@Diameter 0.500 in,
Temperature 842 °F
0.2% offset
Haynes Hastelloy® C-2000® Nickel Alloy Shielded Metal Arc Welded (SMAW) All Weld Cruciform
Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h..
Tensile Strength, Yield 386 MPa

@Thickness 46.1 mm,
Temperature 20.0 °C
56000 psi

@Thickness 1.81 in,
Temperature 68.0 °F
0.2% offset
Haynes Hastelloy® C-22® alloy, transverse, GMAW short arc weldment, plate
HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an..
Tensile Strength, Yield 386 MPa

@Thickness 6.35 mm,
Temperature 20.0 °C
56000 psi

@Thickness 0.250 in,
Temperature 68.0 °F
0.2% offset
Haynes Hastelloy® C-22® alloy, transverse, GTAW weldment, sheet - plate
HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an..
Tensile Strength, Yield >= 386 MPa

@Thickness 3.17 mm
>= 56000 psi

@Thickness 0.125 in
45° Direction
Alcoa 2090-T83 Aluminum
Aluminum-lithium alloy developed for high strength aerospace applications. The Al-Cu-Li alloy offers an 8 per cent density savings when compared with other aerospace alloys. Alloy 2090-T83 also has ..
Tensile Strength, Yield 386 MPa

@Diameter 88.9 mm,
Temperature 25.0 °C
56000 psi

@Diameter 3.50 in,
Temperature 77.0 °F
0.2% offset
Haynes Hastelloy® C-2000® Bar, Annealed at 2100°F (1149°C)
Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h..