Tensile Strength, Yield 384 MPa

@Strain 0.200 %
55700 psi

@Strain 0.200 %
Plate
Haynes 282® Nickel Alloy Sheet, Plate and Bar, Solution Annealed
Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la..