Mechanical Properties Metric English Comments
Tensile Strength, Yield 379 - 552 MPa

@Strain 0.200 %
55000 - 80000 psi

@Strain 0.200 %
Annealed Bar
Schmolz + Bickenbach LeanDupâ„¢ 35N Stainless Steel Bar
Description: LeanDupâ„¢ 35N also known as (Uranus 35 N) is a dual phase austentic-ferritic stainless steel that has the ability to become as important as 316L. It offers better corrosion resistan..
Tensile Strength, Yield 414 - 552 MPa

@Strain 0.200 %
60000 - 80000 psi

@Strain 0.200 %
Cold Drawn Bars
Schmolz + Bickenbach UGIMA 304/304L® Stainless Steel Bar
Description: 304/304L UGIMA® is the next generation of improved high machinability grades from Ugitech. The UGIMA® grades have redefined high machinability stainless steels, showing improvements o..